PCB fabs
A few years ago (not many) I used to burn copper plates using acetic acid, a.k.a. vinegar. I was somewhat concerned about using stronger acids so it was OK to use another acid, even if it was soooo sloooow. If you were patient you could get to have decent boards using 50mil traces (or even thinner). But it required keeping a good temperature on the copper bath and regulating the ratio vinegar/hydrogen peroxide continuously, adding a little salt from time to time to speed things up....